Deep Pour X Epoxy Resin (USA Made by MAS)

Pour up to 3 inches at a time - slow cure time, USA Made, no VOCs....
Part #: MAS-Deep-Pour-X

Deep Pour X is a high-performance epoxy resin casting system formulated with an extra slow cure time allowing up to 3” pours.

This USA Made epoxy resin system is extremely durable, with excellent air release, low exotherm, 100% solids and no VOC’s.

Maintain material and shop temperatures between 60F-80F throughout casting process, cooler is better. This formula is specifically designed for thicker pours, with a minimum recommended casting depth of 2” depending on your working conditions.

Shipping Note: Epoxy Resins can only be transported by UPS Standard - please select that option at checkout.


Click the image to calculate how much epoxy you need!

Note - Epoxy Resins can only be transported by UPS Standard - please select that option at checkout.
Shipping is only available within Continental North America
Specifications

Surface Prep

All surfaces must be clean, dry and free of contami- nation. Contaminates include, but are not limited to dust, oil, moisture, sap, lint, and sanding debris. DO NOT use tack cloth, paper towels, dirty rags, contam- inated sandpaper, or touch surface with oily fingers. Sand as needed and clean off sanding debris. Wipe surface down with a clean cotton t-shirt rag soaked in an oil free solvent like denatured alcohol prior to applying epoxy seal coat. DO NOT apply epoxy over oil based stains.


Mix Epoxy

Mix thoroughly at a 2:1 ratio. 2 parts resin to 1 part hardener (2A:1B) by volume or 100 parts resin to 43 parts hardener (100A:43B) by weight. Using the recommended mix ratio is VERY important. Combine resin and hardener at recommended mix ratio. Mix thoroughly for 5-10 minutes while occasionally scrap- ing sides and bottom of container until no streaks or striations are visible, transfer to a second contain-er, mix 5-10 minutes again until fully blended. Add colored pigment powder or dye to mixture if desired. Before pouring, let fully mixed epoxy dwell in mixing container for 30-45 minutes at 60-80°F to allow release of air bubbles caused by mixing. For larger pours, mix with a drill and paddle mixer.


Pour and Let Cure

Pour epoxy into form and allow epoxy to fully cure for 24-48 hours depending on the thickness. 2” pours or less may take up to 72 hrs to cure.


Physical Properties



Handling Properties


Deep Pour X is a high-performance epoxy resin casting system formulated with an extra slow cure time allowing up to 3” pours.

This USA Made epoxy resin system is extremely durable, with excellent air release, low exotherm, 100% solids and no VOC’s.

Maintain material and shop temperatures between 60F-80F throughout casting process, cooler is better. This formula is specifically designed for thicker pours, with a minimum recommended casting depth of 2” depending on your working conditions.

Shipping Note: Epoxy Resins can only be transported by UPS Standard - please select that option at checkout.


Reviews

Write a Review || | No reviews for this product.

Click the image to calculate how much epoxy you need!

Note - Epoxy Resins can only be transported by UPS Standard - please select that option at checkout.
Shipping is only available within Continental North America

Specifications
Specifications

Surface Prep

All surfaces must be clean, dry and free of contami- nation. Contaminates include, but are not limited to dust, oil, moisture, sap, lint, and sanding debris. DO NOT use tack cloth, paper towels, dirty rags, contam- inated sandpaper, or touch surface with oily fingers. Sand as needed and clean off sanding debris. Wipe surface down with a clean cotton t-shirt rag soaked in an oil free solvent like denatured alcohol prior to applying epoxy seal coat. DO NOT apply epoxy over oil based stains.


Mix Epoxy

Mix thoroughly at a 2:1 ratio. 2 parts resin to 1 part hardener (2A:1B) by volume or 100 parts resin to 43 parts hardener (100A:43B) by weight. Using the recommended mix ratio is VERY important. Combine resin and hardener at recommended mix ratio. Mix thoroughly for 5-10 minutes while occasionally scrap- ing sides and bottom of container until no streaks or striations are visible, transfer to a second contain-er, mix 5-10 minutes again until fully blended. Add colored pigment powder or dye to mixture if desired. Before pouring, let fully mixed epoxy dwell in mixing container for 30-45 minutes at 60-80°F to allow release of air bubbles caused by mixing. For larger pours, mix with a drill and paddle mixer.


Pour and Let Cure

Pour epoxy into form and allow epoxy to fully cure for 24-48 hours depending on the thickness. 2” pours or less may take up to 72 hrs to cure.


Physical Properties